PMID-sentid Pub_year Sent_text comp_official_name comp_offsetprotein_name organism prot_offset 31459640-2 2019 A strong loss of functional groups during pyrolysis at temperatures beyond 300 C of the HTC-derived hydrochars was observed, resulting in an increase of the carbon content up to 95 wt% for the carbon materials pyrolyzed at 800 C and an increase of the specific surface area with a maximum of 520 m2 g-1 at a pyrolysis temperature of 600 C. Devolatilization mainly took place in the range from 300 to 500 C, releasing light pyrolysis gases such as CO, CO2, H2O and larger oxygen-containing molecules up to C11. Carbon 194-200 RNA polymerase III subunit K Homo sapiens 509-512